What is Hastelloy c276 tube ?

Alloy C276 has nickel, chromium and molybdenum in its chemical composition with added tungsten.It shows excellent corrosion resistance in various environments.The Hastelloy C276 tube also shows pitting and crevice corrosion resistance.They have a low carbon content which minimizes the risk of carbon precipitation during welding.The EN 2.4819 square tubing shows good resistance to elevated temperature conditions that can go up to 1038°C.

They possess good mechanical properties, with a minimum yield strength of 345 Mpa.Nickel C276 condenser tubes can achieve strength by undergoing the pilger process.They can also maintain their toughness at cryogenic temperatures.The 2.4819 Hastelloy C276 gas tube can be hot worked within the temperature range of 870-1230 °C.They have a high work hardening rate, so annealing is a recommended process.

Table of content

Most trustworthy hastelloy C276 seamless tube suppliers in India in accordance with ASTM B622, check alloy C276 tube price list

What is the price of alloy c276 tube in India?

The price of alloy C276 tube in India can vary with the suppliers you choose.Firstly, the raw material prices depend on the market conditions and it also changes with the quality.The suppliers also have their internal pricing strategies and the demand for the UNS N10276 cold drawn tube also determines the price.

Now other factors like quantity ordered, added requirements like surface treatments, testings, etc.and delivery location also determine the price.You should always do your research and go for reputed suppliers like Regent Steel & Engineering Co., who offer quality Hastelloy alloy C276 boiler tubes at competitive rates.

We attention to the availability and supply of UNS N10276 heat exchanger tube size range from 12mm to 260 mm and length 6-12 meter with prompt dispatch to Mumbai.see Hastelloy C276 tubing hardness

Alloy c276 tube

Alloy c276 tube

Hastelloy c276 tubing

Hastelloy c276 tubing

UNS N10276 heat exchanger tube

UNS N10276 heat exchanger tube

What is the hardness of Hastelloy c276 tubing?

The hardness value of Hastelloy C276 tubing is 40HRc.Thus, they are suitable for applications that require high strength and resistance to high heat and wear.Hastelloy 2.4819 superheater tubes can be found in industries like chemical and petrochemical processing, pharmaceutical, power generation, pulp & paper production, etc.

Certified stockist of DIN 2.4819 redrawn tube with wall thickness of 1.65mm to 8.18 mm in various shape at a genuine price, know more about specification

Hastelloy c276 tube specification
Size Length Wall Thikness
OD: .125 to 1" 6 to 12 meter .010 to .065 "
Specification Process MTC
ASTM B622/ SB622 seamless, hot rolled, annealed, welded 10204 3.1 & 3.2
Get opportunity to purchase nickel alloy c276 bright annealed tube and superheater tubes for a fair price, check its more available types
List of alloy c276 tube types
Hastelloy c276 seamless tube

Hastelloy c276 seamless tube

  • ASTM B622 | ASME SB622
  • Wall: 010 to .065 inch
  • OD: .125 - 1 inch
DIN 2.4819 redrawn tube

DIN 2.4819 redrawn tube

  • Machining
  • Band Sawing
  • Welding
Nickel alloy c276 bright annealed tube

Nickel alloy c276 bright annealed tube

  • Square
  • Hydraulic
  • Round and rectangular
Any UNS N10276 cold drawn and boiler tubes supply demands can be met by us as one of the leading hastelloy C276 tube suppliers, view its technical properties
DIN 2.4819 redrawn tube chemical properties
Grade Mo C Mn Si Co P S Fe Ni Cr
Hastelloy c276 15.00 – 17.00 0.010 max 1.00 max 0.08 max 2.50 max 0.04 max 0.03 max 4.00 – 7.00 50.99 min* 14.50 – 16.50
UNS N10276 heat exchanger tubes equivalent
STANDARD UNS WERKSTOFF NR. JIS EN GOST OR
Hastelloy c276 N10276 2.4819 NW 0276 NiMo16Cr15W ХН65МВУ ЭП760
Hastelloy c276 seamless tube mechanical properties
Material Hardness Rb Yield Strength (Min) Elongation % C276 filler wire ultimate tensile (min)
Mpa Ksi Mpa Ksi
Hastelloy c276 89 347 50.3 67 741 107.4
Hastelloy c276 86 376 54.6 60 796 115.5
What is the difference between Inconel 625 and Hastelloy c276?
  • Inconel 625 has a high chromium content whereas Hastelloy C276 has higher molybdenum content.
  • 625 shows good oxidation resistance whereas UNS 0276 heat exchanger tube material is reduction resistant.Thus, 625 is preferred in oxidizing environments whereas C276 is for reducing solutions.
What are the disadvantages of Hastelloy C276 seamless tube?
  • The disadvantages of Hastelloy C276 seamless tube will include:
  • C276 is a premium alloy and the seamless tube made from this can be very expensive.
  • It has a specialized composition and is subject to limited availability.This can increase the price of the products and the delivery timelines.
  • nickel alloy C276 bright annealed tube has a high work hardening rate and low thermal conductivity.Thus, they are quite challenging to machine and fabricate.
  • C276 material can get brittle above the temperature of 704 °C.
  • They have a high coefficient of thermal expansion.
  • Hastelloy C276 tube suppliers suggest that the material might not be ideal for all corrosive environments.For example, it can exhibit localized corrosion if exposed to high temperature concentrated sulphuric acid.
Can you weld C276 tubing?

C276 tubing can be easily welded and processed using standard procedures.The hot working temperature for the material is within the range of 870-1230 °C.ERNiCrMo-4 or ERNiCrMo-4 can be used as a filler material in welding DIN 2.4819 redrawn tube for chemical and petrochemical industries.

OD tolerances of alloy C276 tubes
WALL THICKNESS INCHES O.D.INCHES O.D.+/- INCHES
.025 to .065 1 to 1-1/2" incl. .008
Over .065 to .134 .010
.025 to .065 1/2" to 1" incl. .005
Over .065 to .134 .010
.083 to .165 3-1/2" to 5" incl. .020
Over .165 to .220 .025
.032 to .065 2" to 2-1/2" incl. .012
Over .065 to .109 .013
Over .109 to .165 .014
.025 to .049 1-1/2" to 2" incl. .010
Over .049 to .083 .011
Over .083 to .148 .012
.032 to .165 2-1/2" to 3-1/2" incl. .014
Over .165 to .220 .020
Sizes of C276 tubing
Specification Wall Manufacture Method Description OD
ASTM B626 ASME SB626 0.0350 WELDED & DRAWN W HAST C-276 B626 3/8 X .035 WA 0.3750
ASME SB622 0.0360 SEAMLESS & DRAWN SMLS C-276 B622 .375 OD X .065 WA 0.3750
ASTM B626 ASME SB626 0.0650 WELDED & DRAWN W HAST C-276 B626 3/4 X .065 WA 0.7500
ASME SB622 0.0650 SEAMLESS & DRAWN SMLS C-276 B/SB622 .500 OD X .065W 0.5000
ASME SB622 0.0350 SMLS C-276 B622 3/8 X .035 WA 0.3750
ASTM B626 ASME SB626 0.0490 WELDED & DRAWN W HAST C-276 B626 1/2 OD X .049 WA 0.5000
ASTM B626 ASME SB626 0.0490 WDHAST C-276 B626 1/2 OD X .049 WA 0.5000
ASTM B626 ASME SB626 0.0350 W HAST C-276 B626 1/2 X .035 WA 0.5000
ASME SB622 0.0490 SEAMLESS & DRAWN SMLS HAST C-276 B622 1/2 X .049 WA 0.5000
ASME SB622 0.0350 SMLS C-276 B622 1/2 X .035 WA 0.5000
Physical properties of UNS 0276 heat exchanger tubes
Grade Thermal Conductivity (W/m.K) Melting Point °C Density (g/cm3) Co-eff of Thermal Expansion (μm/m/°C) Specific Heat (J/Kg.K)
24-93°C 0-100°C
Hastelloy C276 7.2 1371 8.89 11.2 727
Impact strength of Hastelloy C276 seamless tubes
Test Temperature Impact Strength
°C °F J ft-lbf
-196 -320 519 383
RT RT 479 353
Hastelloy C276 tubes codes
HASTELLOY® C-276
(W10276, N10276)
ASME Section l 1000°F (538°C)1
Code Case 1924 1000°F (538°C)
Section lll
Class 2 800°F (427°C)2
Class 1 -
Class 3 800°F (427°C)2
Section Vlll Div.2 1250°F (677°C)3
Div.1 1250°F (677°C)3
B31.3 1250°F (677°C)7
B16.34 1250°F (677°C)5
B16.5 1250°F (677°C)4
B31.1 1000°F (538°C)6
VdTÜV (doc #) 844°F (450°C)8,
#400
FAQ
What is the speed and feed of Hastelloy C276 seamless tube drilling?

0.004-0.008 in.feed, Speed: 30-50 sfm, 0.150 in depth of cut.

Is alloy C276 tube resistant to hydrochloric acid?

at room temperature it is resistant to all concentrations of hydrochloric acid

What is the maximum working temperature for UNS 0276 heat exchanger tube ?

1800°F (982°C)

What is the corrosion rate of DIN 2.4819 redrawn tube ?

6.47 ± 0.20 mm/y

What are the limitations of nickel alloy C276 bright annealed tube ?

low chromium content